These pores created by SAP work as voids comparable to These generated by AEAs, improving freeze-thaw resistance and toughness. Unlike AEAs, which can eliminate a portion of entrained air due to variables like lengthy hauling durations or high ambient temperatures, SAP's pore system stays steady regardless of consistency, superplasticizer addition, https://nanosiliconpowder58035.wiki-racconti.com/8226862/colored_concrete_powder_an_overview